Well the major glass work on my old tug is beginning and I am quickly running out of warm days. I was hoping one of you glass guys could give me some advise on working with resins in cooler temps.
In the later winter months the daily temps will be in the 40's. I am anticipating the prep getting finished around February and I was hoping I could start glassing at that time. I own a larger boat and I was thinking of tenting the aft end of the boat inclosing it with a tarp and using some heaters. Will this work, or should I wait till spring?
Part of the work will need epoxy while other parts will be poly. (stringers and some bulkheads, maybe some transom supports and backing for a swim platform)
In the later winter months the daily temps will be in the 40's. I am anticipating the prep getting finished around February and I was hoping I could start glassing at that time. I own a larger boat and I was thinking of tenting the aft end of the boat inclosing it with a tarp and using some heaters. Will this work, or should I wait till spring?
Part of the work will need epoxy while other parts will be poly. (stringers and some bulkheads, maybe some transom supports and backing for a swim platform)