Hey everyone im still working away on my Tempest resto haven't had a lot of time to work on it but 2 weekends ago i got the stringers cut and pl'ed in place i glassed them all in on a very hot Sunday and went out Monday to see how it was all going and the glass was still wet and had more air bubbles then not? when i left Sunday it was PERFECT. Then Monday it was a mess it looked like the wood blew all the glass off so i waited 4 days came out it was still wet like it had no hardener. anyways i ground everything i did off and was back to clean wood, tarped the boat and left. then we had a huge rain storm and it blew the tarps off and flooded the boat. the water was in for about 1 day. I finally got there to clean it out and now I'm not sure how long i have to wait for this wood to dry out before i re-glass?? I know why the glass messed up the first time (didnt mix the resin and hardener enough) but how long does this wood have to dry before reglassing? or do i have to rip it out and remake the stringers?